ftc相变节能保温砂浆怎么调配

时间:2016-07-18     作者:www.xzalk.com【原创】   阅读

FTC自调温变相节能保温砂浆材料是以水镁石纤维等无机材料作为骨架材料,合理选用并添加相变材料,经科学配比及特殊工艺复合而成,且有保温、隔热、防火、隔声等功能。

FTC from air-conditioning energy-saving insulation mortar material is disguised brucite fibers such as inorganic materials as skeleton material, a reasonable choice and add a phase change material, compounded by scientific proportioning and special process, and have heat preservation, heat insulation, fire prevention, sound insulation, and other functions.


FTC自调温变相节能保温砂浆适用于各种砖混结构、框架和剪力墙结构建筑的外墙复合保温及地下室、车库、楼梯走廊等公共设施的防火保温。

FTC from tempering disguised energy-saving insulation mortar are suitable for all kinds of composite masonry structure, frame and shear wall structure construction compound heat preservation and the exterior wall of basement, garage, fire insulation staircase corridor and other public facilities。


FTC自调温变相节能保温砂浆施工环境温度5℃~35℃,阳光曝晒下和大风雨天不宜施工。

FTC from tempering disguised energy-saving insulation mortar construction environment temperature 5 ℃ ~ 35 ℃, and winds rain unfavorable construction when exposed to sunlight.


调制方法

Modulation method


成品料 :水=(0.85-1): 1左右(质量比) ,砂浆不宜搅拌得过稀。用搅拌器搅拌均匀静置3分钟后,再次搅拌即可使用。

Finished product: water = (0.85 1) : 1 (mass ratio), mortar shoulds not be too thin. Using blender mixing uniform stand for 3 minutes, stirring can be used again.


注意事项

Matters needing attention


调制浆料时只加水,不得添加其它骨料、砂、添加剂等。配好的浆料应在3小时内用完。

Modulation slurry when just add water, can not add other aggregate, sand and additive, etc. With good size should be finished within 3 hours.

以下产品    详细咨询18832673888   进入网站查看详细情况

 

保温砂浆 www.xzalk.com

硅酸盐板

阿里巴巴华东官网

阿里巴巴华东分店 huadong。1688。com


最新评论
请先登录才能进行回复登录
  • 电话直呼

    • 18831662333
    • 销售经理 :
    • 售前咨询 :
    • 售前咨询 :
    • 售后服务 :
    • 售后服务 :
    • 合同签订/施工方案 :
    • 合同签订/施工方案 :
  • 扫一扫,关注旺铺

上海快3开奖记录 上海快3走势图 上海快3 上海快3 上海快3走势图 上海快3走势图 上海快3 上海快三基本走势图50期 上海快3走势图 上海快3走势图